The addition of initiator affects the crossover point of the storage modulus (solid line) and the loss modulus (dashed lined), which indicates curing. As initiator content increases, the reaction proceeds more quickly.

The approach is to use peroxides to modify the reaction kinetics in the production of polysiloxanes.  A radical initiator in the presence of a hydride-terminated polysiloxane will increase the rate of curing and reduce manufacturing costs.  At a minimum a formulation would contain a hydride-terminated polysiloxane, a platinum catalyst, and an initiator that generates radicals.  The content of…

Image
Plasma wind
CRETIN is a 1D, 2D, and 3D non-local thermodynamic equilibrium (NLTE) atomic kinetics/radiation transport code which follows the time evolution of atomic populations and photon distributions as radiation interacts with a plasma consisting of an arbitrary mix of elements. It can provide detailed spectra for comparing with experimental diagnostics.